Semi-crystalline thermoplastic PEEK film filled with 20 % talc
General properties:
- higher thermal conductivity
- lower thermal expansion coefficient
- higher modulus of elasticity
Physical properties:
- Density (ISO1183): 1,45 g/cm³
- Glass transition temperature (ISO11357): 143 °C
- Melting temperature: 343 °C
Mechanical properties: (sample thickness 50 µm)
- Tensile strength at 23°C (ISO527): 98 N/mm²
- Tensile elongation at 23°C (ISO527): 25 %
- Tensile modulus (ISO527): 5300 N/mm²
Thermal properties:
- Thermal expansion coefficient x 10³, T<Tg: 0,023 1/°K
- Thermal conductivity x 10² (DIN52612): 37 W/mK